Item | Name | Tel | |
---|---|---|---|
Color-tinted | Jung Hoon, Jung | 82-2-3787-1654 | xquakerx@sk.com |
SKC’s color-tinted film is a polyester film made by the chip-dyed processing method of making films after color application to the transparent chip that is used as raw material for the film. With a uniform and vivid color, it is mainly used as the base film for window films of vehicles and construction.
Major products | Features |
---|---|
ST16K | VLT 4%~17%, Black Colored film, Color-tinted film coated with urethane primer and corona |
ST36K | VLT 29%~33%, Black Colored film, Color-tinted film coated with urethane primer and corona |
ST51K | VLT 37%~43%, Black Colored film, Color-tinted film coated with urethane primer and corona |
Property | Unit | Value | Test Method | |||||
---|---|---|---|---|---|---|---|---|
ST16K | ST16K | ST36K | ST51K | |||||
General | Nominal | Gauge | 92 | 144 | 92 | 92 | SKC Method | |
Thickness | ㎛ | 23 | 36 | 23 | 23 | |||
Mechanical | Tensile | Kg/㎟ | MD | 22.5 | 22.7 | 21.5 | 22.7 | ASTM D 882 |
Strength | TD | 28.5 | 28.0 | 27.7 | 28.7 | |||
Elongation | MD | 190 | 188 | 198 | 188 | ASTM D 882 | ||
At Break | TD | 131 | 129 | 132 | 130 | |||
Surface | Surface Tension | dyne/㎝ | Corona | 54 | 54 | 54 | 54 | ASTM D 2578 |
Optical | Haze | % | 0.8 | 0.9 | 0.7 | 0.7 | ASTM D 1003 | |
Light Transmission |
% | 16 | 6 | 30 | 39 | EDTM SD2400 | ||
Thermal | Heat | % | MD | 1.3 | 1.3 | 1.2 | 1.3 | SKC Method (150℃×30 min) |
Shrinkage | TD | 0.0 | 0.3 | 0.0 | 0.1 |